Phosphate-bonded crown and bridge investment material for rapid heating
For non-precious and precious metal alloys as well as rapid heating
- low-priced alternative for reliable casting results
- thermally resilient
- also classic, gradual preheating possible
Technical data Mixing ratio 22 ml liquid : 100 g powder Setting time 30 min (22 °C) Pre-heating Speed | gradual with retention times End temperature 650 - 900 °C Total expansion 3.3% (100 % conc.)
4.5 kg (30 x 150 g bags)
PRICE INCLUDES LIQUID