Phosphate-bonded crown and bridge investment material for rapid heating
For non-precious and precious metal alloys as well as rapid heating
- excellent flow behaviour and long processing time
- very soft during deflasking high expansion liquid available
- also classic, gradual preheating possible
Technical data
Mixing ratio 28 ml liquid : 100 g powder
Setting time 30 min (22 °C)
Pre-heating Speed | gradual with retention times
End temperature 650 - 900 °C
Total expansion 3.1 % (100 % conc.)
PRICE DOES NOT INCLUDE LIQUID
Click here to buy the liquid